Article citationsMore >>

T. Hino, J. Chai, T. Negami, D. Bergado and R. Jia, "Assessment of the Effects of Sea-level Change on the Geoenvironment: the Case of the Ariake Costal Lowland.," in ¬9th International Symposium on Lowland Technology, September 29-October 1, 2014 in Saga, Japan., Saga, 2014.

has been cited by the following article:

Article

Influence of Water-Cement Ratio on the Strength Distribution inside a Soil-Cement Material

1Department of Civil Engineering and Architectural Design, Saga University, Saga, Japan

2Ministry in charge of infrastructures, Ouagadougou, Burkina Faso

3Faculty of Exact and Applied Sciences (UFR-SEA), University Joseph Ki-Zerbo, Ouagadougou, Burkina Faso

4Department of Civil Engineering, Yokohama National University, Yokohama, Japan


American Journal of Civil Engineering and Architecture. 2024, Vol. 12 No. 2, 24-29
DOI: 10.12691/ajcea-12-2-1
Copyright © 2024 Science and Education Publishing

Cite this paper:
Donzala D. Some, Ohindemi G. Yameogo, Magai N. Thon. Influence of Water-Cement Ratio on the Strength Distribution inside a Soil-Cement Material. American Journal of Civil Engineering and Architecture. 2024; 12(2):24-29. doi: 10.12691/ajcea-12-2-1.

Correspondence to: Donzala  D. Some, Department of Civil Engineering and Architectural Design, Saga University, Saga, Japan. Email: donzdavids@gmail.com

Abstract

In the domain of soil-cement, especially within the deep mixing method (DMM), various factors influence the strength of cement-stabilized soft soils. These factors include soil candidate consistency parameters, cement content, water-cement ratio (W/C), mixing time, and curing time. Notably, a lower W/C ratio resulted in a higher unconfined compressive strength (qu). However, in the context of improving soft and cohesive soils through DMM, a W/C ratio of 1.0 has conventionally been recommended due to its favorable resistance. In the case of the Saga lowland, where a soft cohesive soil with high compressibility and low strength is prevalent, the standard practice employs a W/C ratio of 1.0 with a selective amount of cement for different layers, in most projects. This research introduces an innovative approach: utilizing a higher W/C ratio of 1.5 with a cement content of 110 kg/m³, to fulfill the standard strength requirement and above all, to have a well-distributed strength inside the material. This could prevent the lateral displacement of the soil-cement columns. Through laboratory experiments, this paper investigates the effects of increasing W/C on the strength distribution. As result, the comparison between the needle penetration strength (qunp) /C= 1 and 1.5 showed that the latter represents a slight reduction in strength, but it is more uniformly distributed. This approach is designed to a bolster support for the existing infrastructure in the Saga lowland. The significance of this study in the field of DMM lies in advocating for an increased W/C ratio to ensure not only the quality of the mixture but also, more importantly, the uniformity of strength within the soil-cement columns.

Keywords